چکیده مقاله
This study evaluates the effectiveness of dry and wet magnetic separation techniques, integrated with magnetizing roasting, for enhancing iron recovery from low-grade iron tailings (32.5% Fe). The primary objective is to develop a process for upgrading a large tailings deposit into a marketable product (≥60% Fe grade). Mineralogical analysis revealed that the sample primarily comprises magnetite, hematite, and goethite as iron-bearing minerals, with silicates and carbonates as the main gangue phases. Dry magnetic separation tests indicated that, under optimal conditions, a concentrate with 53.21% Fe content, 52.34% mass recovery, and 85.01% iron recovery could be achieved. The sample was ground, classified into size fractions, and subjected to wet magnetic separation. Wet magnetic separation tests demonstrated that a concentrate assaying 61.5% Fe could be obtained through rougher-cleaner beneficiation of the -100 µm fraction using a 1200 G magnetic field and a 30% slurry solids concentration. Magnetizing roasting of the rougher tailings further produced a concentrate containing 57.24% Fe with an iron recovery of 54.93%. Based on the results obtained, a process was developed for the beneficiation of low-grade magnetite-hematite tailings.
لینک ثابت مقاله